Our well-equipped facilities and great excellent command throughout all stages of generation enables us to guarantee total customer fulfillment for 16mm Mineral Fiber Ceiling Tiles 16mm , Heat Insulation Board , Acoustic Ceiling , Our products enjoy good popularity among our customers. We welcome customers, business associations and friends from all parts of the world to contact us and seek cooperation for mutual benefits.
Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose HPMC – Beihua Detail:

In building materials, it is used as a water-retaining agent and retarder for cement sludge with pumpability. It can be used as a binder in plaster, gypsum, inverted powder or other building materials to improve spreadability and prolong operation time. It can be used as an agent for sticking bricks, tiles, marbles, plastic decorations, and bonding intensifiers. It can also reduce the amount of cement. The water retention of HPMC prevents the slurry from cracking due to drying too fast after coating, and enhances the strength after hardening.

In addition, it is used as thickener, stability, emulsifier, excipient, water retention in the production of other petrochemicals, coatings, building materials, paint removers, agricultural chemicals, inks, textile printing and dyeing, ceramics, papermaking, and cosmetic brands. Agent, film-forming agent, etc.

1. Appearance: white or almost white powder, odorless and tasteless.

2. Granularity: 10 mesh pass rate is greater than 98.5%; 80 mesh pass rate is greater than 100%.

3. Carbonization temperature: 280-300℃.

4. Room density: 0.25-0.7G/CM3 (usually about 0.5G/CM3), the specific gravity is 1.26-1.31.

5. Discoloration temperature: 190-200℃.

6. Natural temperature: about 360℃.

 

Production Method

The refined cotton cellulose is treated with lye at 35-40°C for half an hour, squeezed, the cellulose is crushed, and properly aged at 35°C, so that the obtained alkali fiber average degree of polymerization is within the required range. Put the alkali fiber into the etherification kettle, add propylene oxide and methyl chloride successively, and etherify at 50-80℃ for 5h, the maximum pressure is about 1.8MPa. Then add proper amount of hydrochloric acid and oxalic acid to wash materials in hot water at 90°C to increase the volume. Dehydrate with a centrifuge. Wash to neutral. When the water content in the material is less than 60%, dry it with a stream of hot air at 130℃ to less than 5%. Finally, it is crushed through a 20-mesh sieve to obtain the finished product.

 


Product detail pictures:

Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose  HPMC – Beihua detail pictures


Related Product Guide:

As a way to present you with ease and enlarge our enterprise, we also have inspectors in QC Workforce and assure you our greatest support and solution for Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose HPMC – Beihua , The product will supply to all over the world, such as: Netherlands, India, Malta, All of our products comply with international quality standards and are greatly appreciated in a variety of markets around the world. If you are interested in any of our products or would like to discuss a custom order, please feel free to contact us. We are looking forward to forming successful business relationships with new clients in the near future.
  • We have been engaged in this industry for many years, we appreciate the work attitude and production capacity of the company, this is a reputable and professional manufacturer.
    5 Stars By Claire from Montpellier - 2017.10.27 12:12
    After the signing of the contract, we received satisfactory goods in a short term, this is a commendable manufacturer.
    5 Stars By Prudence from Qatar - 2017.12.31 14:53
    Write your message here and send it to us